MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Chemlon® MD21 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Notes: MD32 is a medium viscosity grade of nylon 6 designed for wire coating extrusion. MD21 is heavily pigment and is designed to provide good opacity even with thin coatings. It also features a lubrication system that is designed to ensure excellent adhesion between the wire and the coating- as well as optimal processing characteristics at high line speeds. MD21 is available in range of colors – including heavy metal free options.

Availability: Europe; North America

Additive: Lubricant

Features: Good Adhesion; Good Processability; Lubricated

Uses: Wire & Cable Applications; Wire Jacketing

Form: Pellets

Processing Method:Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 - 1.38 g/cc0.0412 - 0.0499 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus 3.00 - 3.60 GPa435 - 522 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 - 95.0 °C185 - 203 °FUnannealed; ISO 72-2/A
 
Processing PropertiesMetricEnglishComments
Zone 1 250 - 300 °C482 - 572 °F
Zone 3 250 - 300 °C482 - 572 °F
Zone 5 250 - 300 °C482 - 572 °F
Melt Temperature <= 300 °C<= 572 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 2.00 hour2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0580 / 237071

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.