MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled

Material Notes: Ultramid 8231G HS BK-102 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffness and heat deflection temperature. The heat stabilizer system extends the properties at elevated temperatures. It also has excellent chemical resistance to greases, oils and hydrocarbons.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³dry; ISO 1183
Water Absorption 1.4 %1.4 %24 hour; ISO Test
 8.1 %8.1 %beginning dry; ISO 62
Moisture Absorption at Equilibrium 2.3 %2.3 %beginning dry (23°C/50% R.H.); ISO 62
Relative Viscosity 2.6 cP2.6 cPISO Test; 96 % SAV
Viscosity Measurement 5050Formic Acid
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psi0.2 in/min; ASTM Test
 30.0 MPa
@Temperature 80.0 °C
4350 psi
@Temperature 176 °F
ISO Data
 30.0 MPa
@Temperature 80.0 °C
4350 psi
@Temperature 176 °F
ASTM Test
 40.0 MPa
@Temperature 120 °C
5800 psi
@Temperature 248 °F
ASTM Test
 40.0 MPa
@Temperature 120 °C
5800 psi
@Temperature 248 °F
ISO Data
 150 MPa
@Temperature -40.0 °C
21800 psi
@Temperature -40.0 °F
ISO Data
 150 MPa
@Temperature -40.0 °C
21800 psi
@Temperature -40.0 °F
ASTM Test
Tensile Strength, Ultimate 60.0 MPa8700 psi5mm/min; ISO 527
Elongation at Break 20 %20 %5mm/min; ISO 527
 20 %20 %0.2 in/min; ASTM Test
 3.0 %
@Temperature -40.0 °C
3.0 %
@Temperature -40.0 °F
ASTM Test
 3.0 %
@Temperature -40.0 °C
3.0 %
@Temperature -40.0 °F
ISO Data
 9.0 %
@Temperature 120 °C
9.0 %
@Temperature 248 °F
ISO Data
 9.0 %
@Temperature 120 °C
9.0 %
@Temperature 248 °F
ASTM Test
 15 %
@Temperature 80.0 °C
15 %
@Temperature 176 °F
ASTM Test
 15 %
@Temperature 80.0 °C
15 %
@Temperature 176 °F
ISO Data
Tensile Modulus 3.10 GPa450 ksi1mm/min; ISO 527
 1.80 GPa
@Temperature 120 °C
261 ksi
@Temperature 248 °F
ISO Data
 2.30 GPa
@Temperature 80.0 °C
334 ksi
@Temperature 176 °F
ISO Data
 6.90 GPa
@Temperature -40.0 °C
1000 ksi
@Temperature -40.0 °F
ISO Data
Flexural Strength 65.0 MPa9430 psiISO Data
Flexural Modulus 2.21 GPa321 ksiISO Data
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 °C527 °FInjection molding
Mold Temperature 95.0 °C203 °FInjection molding
 
Descriptive Properties
ColorBK-102
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicHeat stabilized or stable to heat
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Dry)
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry)
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Conditioned)
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Conditioned)
BASF Ultramid® 8231G HS BK-106 14% Glass Filled PA6 (Dry)

PBASF9154 / 84918

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.