MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil 222 Mobilgrease FM
Categories: Fluid; Lubricant; Aluminum Gellant

Material Notes: Mobilgrease FM 221 and FM 222 are high performance multi-purpose products designed specifically for the lubrication of food processing machinery. Mobilgrease FM 221 and FM 222 are formulated with components meeting the requirements of CFR 178.3570, Chapter 21, and are NSF registered as H1 classified lubricants. Food processing equipment often operates in a variety of environments, covering the extremes of temperatures from oven to freezer operations, as well as a high level of contamination from water, steam and cleaning agents. Mobilgrease FM 221 and FM 222 were developed as mid-viscosity, multipurpose grease lubricants capable of providing excellent lubrication in all of these environments. Mobilgrease FM 221 and FM 222 are engineered with excellent water resistance to withstand periodic washdown and cleaning operations frequent in the food processing industry. Rust inhibition is a critical property for the industry. Mobilgrease FM 221 and FM 222 are formulated with an excellent rust inhibition package which, working in concert with the water resistance properties, will provide protection against rust. The ISO VG 220 base oil viscosity coupled with excellent thickener shear stability translates into an ability to provide lubrication over a wide range of speeds, loads and temperatures. Mobilgrease FM 221 and FM 222 are also formulated to handle a variety of loads, exhibiting good protection against wear and shock load conditions. Mobilgrease FM 221 and FM 222 were designed to meet many global performance and cultural requirements, including: HSF H1 Registered; DIN 51825 KPF1K -20 (for Mobilgrease FM 221); DIN 51825 KPF2K-20 (for Mobilgrease FM 222); Kosher/Parve; Halal

Mobilgrease FM 221 and FM 222 greases are recommended for multi-purpose lubrication of food processing equipment where NSF H1 registration is required. The food industry includes food processing, beverage, medical and packing industries for a wide range of cultures. Applications include: General rotating equipment lubrication; Conveyor bearings; Equipment central lubrication systems (FM 221); Anti-friction roller bearings under heavy or shock loading; Linkages and slides; Joints

Key Words: NLGI Grade 2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Kinematic Viscosity at 40°C (104°F) 220 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 315 kgASTM D2596
Four Ball Wear 0.500 mmASTM D2266
Penetration 5.0Penetration Consistency Change, 100000 Stroke, Change from Worked Pen, mm/10; ASTM D1831
 280Worked, 25°C, mm/10; ASTM D217
 
Thermal PropertiesOriginal ValueComments
Dropping Point 260 °CASTM D2265
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Colorwhite
Copper Strip Corrosion, ASTM D40481B
Corrosion Prevention, ASTM D1743pass
Grease Life, DIN 51821 (FE-9), hours100 (min)@ 120°C
Soap/Thickener Typealuminum complex

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil 220 Mobilith SHC Series
ExxonMobil 220 Mobilith SHC PM

WEXXON408 / 75833

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.