MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ixom Alkamix™ MB-AO300 Additive Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: ALKAMIX™ MB-AO300 is BHT (Butylated Hydroxy Toluene) free antioxidant masterbatch designed to impart thermal processing stability to base grade low density polyethylene during extrusion. ALKAMIX™ MB-AO300 can be added to base grade low density polyethylene during extrusion to assist in overcoming thermal instability problems. The level required will vary according to the type of extrusion, conditions and polymer used, however the recommended addition level is between 1 and 2 percent. ALKAMIX™ MB-AO300 can also be used as a shutdown compound to prevent oxidation of polymer left idle in an extruder. As a shutdown compound, it is usually added at concentrations of 30 percent or more to fractional MFI low density polyethylenes. The maximum level of addition of ALKAMIX™MB-AO300 based on both good manufacturing practice and to ensure conformance to the requirements to the United States Food and Drug Administration Regulations CFR21 is 4 percent, when added to a polyethylene formulation free of any other additives. The suitability of finished articles manufactured using this material as a component, and the observance of given limitations, must be verified by the converter for each application to ensure compliance with all relevant regulations. An overall migration limit may apply to the finished article.

Information provided by Ixom Operations PTY LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 °C392 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PIXOM004 / 283085

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.