Properties: ATBC is almost colourless and odourless oily liquid, free of foreign materials which is in soluble in water but soluble in alcohols and organic solvents and is miscible and compatible with all the monomeric plasticizers of PVC compounding. Application: 1. Main plasticizer of polyvinyl chloride for food packing and medical products. 2. Main plasticizer of vinyl chloride - vinyldene chloride copolymer for food packing and precise instrument packing. 3. Plasticizer of vinyl chloride - acetate copolymer. 4. Plasticizer of sustained-release pharmaceutical tablets. 5. Plasticizer of latex adhesives. 6. Lubricating oil for surface treatment of tinplate. 7. In manufacturing of toys and safety glasses. Chemical Name: 2-acetyl-1,2,3-Propane tri carboxylic acid Tributyl Ester Molecular Formula: C 20 H34 O8 CAS Number: 77-90-7 EINECS NO.: 201-070-7 Information provided by KLJ Group |