MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sika AcouBond®-System Elastic Bonding and Acoustical Dampening
Categories: Other Engineering Material

Material Notes: The Sika AcouBond-System incorporates Direct Bond Technology with acoustic performance. The Sika AcouBond-System consists of SikaLayer-03, a 1/8” (3 mm) proprietary specially slotted foam mat, and the SikaBond-T53, unique permanently elastic, super strong, sound dampening adhesive that form a tenacious bond to wood flooring, plywood subfloors, concrete and other common subfloor materials

Uses: The Sika AcouBond-System is used to bond structurally sound solid and engineered hardwood in new construction and renovations in residential, office, and industrial buildings as well as sales and show rooms. It is commonly used over in-floor radiant heating and on grade cement and gypsum-based slabs. Field testing demonstrates unmatched sound reductions.

Advantages:

  • Independently tested to – FIIC 59 and FSTC 59
  • Extremely easy to install
  • Structurally bonds wood flooring to subfloor
  • SikaBond-T53 bonds solid wood flooring up to 8 in. (18 cm) wide and engineered planks up to 14 in. (36 cm) wide directly to concrete substrates. No limitations on maximum wood length.
  • Eliminates the extensive labor of installing cork underlayments
  • No need for sleepers and plywood over concrete- and gypsum-based subfloors
  • Innovative walk-on work method
  • Can reduce overall installation costs up to 30%
  • Suitable for bonding wood floors directly onto old ceramic tiles
  • Reduces stress on the substrate

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.87 g/cc0.0676 lb/in³with SikaLayer-03
Volatile Organic Compounds (VOC) Content 48.3 g/l48.3 g/lwith SikaBond-T53
Thickness 3000 microns118 milwith SikaLayer-03
Storage Temperature 10.0 - 25.0 °C50.0 - 77.0 °Fwith SikaLayer-03
 10.0 - 25.0 °C50.0 - 77.0 °Fwith SikaBond-T53
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 404028 days at 73°F(23°C) and 50% RH, with SikaBond-T53
Tensile Strength 1.20 MPa174 psicured at 73°F(23°C) and 50% RH, with SikaBond-T53
Elongation at Break 500 %500 %cured at 73°F(23°C) and 50% RH, with SikaBond-T53
Shear Strength 1.20 MPa174 psi1 mm adhesive thickness at 73°F(23°C) and 50% RH, with SikaBond-T53
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0420 W/m-K0.291 BTU-in/hr-ft²-°Fwith SikaLayer-03
Maximum Service Temperature, Air 70.0 °C158 °Fsuitable for in-floor radiant heating, with SikaBond-T53
Minimum Service Temperature, Air -40.0 °C-40.0 °Fsuitable for in-floor radiant heating, with SikaBond-T53
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min
@Thickness 3000 mm
24.0 hour
@Thickness 118 in
50% RH, with SikaBond-T53
Tack-Free Time 45.0 - 60.0 min0.750 - 1.00 hour50% RH, with SikaBond-T53
 
Descriptive Properties
Chemical BasePolyethylene foamwith SikaLayer-03
ColorGraywith SikaLayer-03
 Whitewith SikaBond-T53
Footfall Sound Reduction<24 dBwith SikaLayer-03

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Exxtra™ Seal POP 4573 Plastomer for Elastic Film and Elastic Film Blends
Armacell OleTex® BDJN 200 EVA/LDPE Foam
3D Systems FabPro™ Elastic BLK Elastomer
Sika Level Rapid Patch Fast-setting cementitious patch
ExxonMobil Escorene® LD-728 High EVA Resin

PSIKA901 / 209808

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.