MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Radici Radilon® A RV350HHR 3800 BK Polyamide 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: PA66 35% glass fiber filled, injection molding grade with enhanced thermal resistance in contact with hot air. High improvement of mechanical properties retention versus standard polyamide 66 after heat aging. Alternative to PPA and PA4.6 grades in automotive applications like turbo air ducts, CAC tanks, EGR housing. Continuous use temperature until 210°C in air.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³DAM; ISO 1183
Water Absorption 6.3 %
@Thickness 2.00 mm,
Temperature 23.0 °C
6.3 %
@Thickness 0.0787 in,
Temperature 73.4 °F
Immersion; ISO 62
Moisture Absorption 1.50 %
@Thickness 2.00 mm,
Temperature 23.0 °C
1.50 %
@Thickness 0.0787 in,
Temperature 73.4 °F
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psi5mm / min. Conditioned; ISO 527-2/1A
 170 MPa24700 psi5mm / min. DAM; ISO 527-2/1A
Elongation at Break 3.5 %3.5 %5 mm / min. DAM; ISO 527-2/1A
 6.5 %6.5 %5 mm / min. Conditioned; ISO 527-2/1A
Tensile Modulus 7.60 GPa1100 ksi1mm / min. Conditioned; ISO 527-2/1A
 10.5 GPa1520 ksi1mm / min. DAM; ISO 527-2/1A
Flexural Strength 190 MPa27600 psi2mm / min. Conditioned; ISO 178
 265 MPa38400 psi2mm / min. DAM; ISO 178
Flexural Modulus 7.00 GPa1020 ksi2mm / min. Conditioned; ISO 178
 9.40 GPa1360 ksi2mm / min. DAM; ISO 178
Charpy Impact Unnotched  9.00 J/cm²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 9.50 J/cm²
@Temperature -30.0 °C
45.2 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 9.50 J/cm²
@Temperature -30.0 °C
45.2 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  1.40 J/cm²
@Temperature -30.0 °C
6.66 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 1.60 J/cm²
@Temperature -30.0 °C
7.61 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1e/A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned. 500V; IEC 60093
 1.00e+13 ohm-cm1.00e+13 ohm-cmDAM; 500V.; IEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmConditioned. 500V; IEC 60093
 1.00e+12 ohm1.00e+12 ohmDAM; 500V.; IEC 60093
Comparative Tracking Index 350 V350 VDAM. Sol.A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F10°C/min; ISO 11357-1/-3
Hot Ball Pressure Test >= 160 °C>= 320 °FIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °FISO 75/2Af
Flammability, UL94 HBHB
Glow Wire Flammability Index 700 °C
@Thickness 2.00 mm
1290 °F
@Thickness 0.0787 in
IEC 60695-2-1/2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FInjection Molding
Mold Temperature 80.0 - 100 °C176 - 212 °F
 
Descriptive Properties
Injection Molding Injection SpeedMedium - high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADI6926 / 293431

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.