Description: LUTENE BB0808 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of shrink film and pallet shrink covers. LUTENE BB0808 have the balanced shrink properties and good clarity make suitable for shrink film. (LUTENE BB0808 contains neither slip agent nor antiblock agent.) Main Application: Shrinkage film, Pallet shrink cover, chopping board, All types of industrial packing CAS No. 9002-88-4 Information provided by LG Chemical |