MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Primef® 4002 40% GF PPS, High Fluidity Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced

Material Notes: Used for injection molding of high performance parts.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.61 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cmSolvay Test Method
Spiral Flow 25.0 cm
@Temperature 300 °C
Solvay Method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 160 MPaISO 527
Elongation at Break 1.6 %ISO 527
Tensile Modulus 13.0 GPaISO 527
Flexural Strength 225 MPaISO 178
Flexural Modulus 13.0 GPaISO 178
Izod Impact, Notched 65.0 J/mISO 180
Izod Impact, Unnotched 2.50 J/cmISO 180
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cmIEC 93/167
Dielectric Constant 3.9
@Frequency 1e+6 Hz
IEC 250
 4.0
@Frequency 1000 Hz
IEC 250
Dielectric Strength 17.0 kV/mmIEC 243
Dissipation Factor 0.0020
@Frequency 1000 Hz
IEC 250
 0.0020
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 150 VIEC 112
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.500 W/m-KISO 8302
Melting Point 280 °C
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °CISO 75
Glass Transition Temp, Tg 90.0 °C
Flammability, UL94 V-0
@Thickness 0.800 mm
Oxygen Index 52 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 320 - 350 °C
Melt Temperature 320 - 330 °C
Mold Temperature 150 - 160 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese FORTRON® 9140L4 40% Glass Reinforced Polyphenylene Sulfide (PPS)
Syensqo (Solvay Specialty Polymers) Primef® 7002 Polyphenylene Sulfide (PPS), 65% Glass\Mineral
Syensqo (Solvay Specialty Polymers) Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement
Celanese FORTRON 1140LC6 PPS, 40% Specialty

PSOL8Z220 / 101374

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.