MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics PZT 400 Series PZT 406 Piezo Ceramic  (discontinued **)
Categories: Ceramic; Piezoelectric

Material Notes: Hard PZT, Navy type I, EN 50324-1: 100.

Information provided by Morgan Advanced Materials. Morgan's electroceramic business was sold to Ceramtec in 2018.

Key Words: PZT 400 Series
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Poissons Ratio 0.300.30
 
Electrical PropertiesMetricEnglishComments
Curie Temperature 325 °C617 °F
Dielectric Constant 13251325KT33
Dielectric Loss Index 0.350.35
Piezoelectric Longitudinal Coupling Factor, k33 0.700.70
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V 130130
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 26.926.9
Piezoelectric Planar Coupling Factor, kp 0.610.61
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 315315
Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N 11.111.1
Piezoelectric Transverse Coupling Factor, k31 0.340.34
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 160 °C320 °F
 
Descriptive Properties
Piezoelectric PropertiesHz-m Frequency Constant (N3t)
 Hz-m Frequency Constant (Np)
Time StabilityAging Rate- coupling -2.5% per decade
 Aging Rate- Dielectric -6.0% per decade
 Aging Rate- frequency 0.5% per decade

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics PZT 400 Series PZT 403 Piezo Ceramic
Morgan Advanced Ceramics PZT 400 Series PZT 407 Piezo Ceramic
Morgan Advanced Ceramics PZT 400 Series PZT 402 Piezo Ceramic
Morgan Advanced Ceramics Piezo Materials for Medical Devices PZT-5A Piezoceramic Material
Morgan Advanced Ceramics High Performance Piezo PZT-5H Piezoelectric Material

CMORF5044 / 200282

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.