MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Prodways PLASTCure Model 300 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: High accuracy and excellent resolution. Ability to produce sharp edges and detailed parts. High green strength and good mechanical properties.

Applications: Broad range of dental model applications. Suited for thermoforming applications

Information provided by Genistar.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Water Absorption 0.60 - 0.80 %0.60 - 0.80 %ASMT D570
Viscosity 350 - 550 cP
@Temperature 23.0 °C
350 - 550 cP
@Temperature 73.4 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 85 - 9085 - 90
Tensile Strength 72.0 - 76.0 MPa10400 - 11000 psiASTM D638
Elongation at Break 5 - 7.0 %5 - 7.0 %ASTM D638
Tensile Modulus 2.80 - 7.00 GPa406 - 1020 ksiASTM D638
Flexural Strength 110 - 120 MPa16000 - 17400 psiASTM D790-10
Flexural Modulus 2.30 - 2.60 GPa334 - 377 ksiASTM D790-10
Flexural Strain at Break 8.0 - 10 %8.0 - 10 %ASTM D790-10
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 - 76.0 °C162 - 169 °FASTM D648
 
Descriptive Properties
AppearanceReddish beige

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DSM Somos® BioClear
3D Systems DuraForm® PA Nylon for SLS® Systems
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems
MicroFine™ Protoyping Resin
DSM Somos® ProtoTherm™ 12110 Water-resistant resin for stereolithography, Thermal Postcure

PPRODW902 / 172308

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.