MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Sandvik Bioline High-N Tube and pipe, seamless
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Sandvik Bioline HighN is a molybdenum and nitrogen alloyed austenitic stainless steel characterized by:
  • A proof strength up to twice that of Sandvik Bioline 316LVM in annealed condition
  • Higher corrosion resistance than Sandvik Bioline 316LVM
  • High micro-cleanliness
  • High surface finish
  • Good forgeability
Sandvik Bioline HighN is used by customers for orthopedic implants and fracture fixation devices.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 740 MPaBar, Annealed
 >= 740 MPaTube, thick wall, Bright annealed
 >= 1000 MPaBar, Medium
 >= 1100 MPaBar, Hard
 >= 1200 MPaTube, thick wall, Cold finished
 <= 1500 MPaWire
Tensile Strength, Yield >= 430 MPa
@Strain 0.2 %
Tube, thick wall, Bright annealed
 >= 430 MPa
@Strain 0.2 %
Bar, Annealed
 >= 700 MPa
@Strain 0.2 %
Bar, Medium
 >= 1000 MPa
@Strain 0.2 %
Bar, Hard
 >= 1100 MPa
@Strain 0.2 %
Tube, thick wall, Cold finished
Elongation at Break 10 %Bar, Hard
 20 %Bar, Medium
 35 %Bar, Annealed
 >= 62 %Tube, thick wall, Bright annealed
Modulus of Elasticity 200 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.5 µm/m-°C
@Temperature 30.0 - 100 °C
Specific Heat Capacity 0.485 J/g-°C
Thermal Conductivity 14.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.060 %
Chromium, Cr 20.5 %
Copper, Cu <= 0.20 %
Manganese, Mn 4.0 %
Molybdenum, Mo 2.4 %
Nickel, Ni 9.5 %
Niobium, Nb (Columbium, Cb) 0.30 %
Nitrogen, N 0.40 %
Phosphorus, P <= 0.025 %
Silicon, Si <= 0.060 %
Sulfur, S <= 0.0030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carpenter 18-18 Plus Austenitic Stainless Steel Composition Spec
Kinetics MIM 316 Stainless Steel (Premium Grade)
EMS-Grivory Grilamid® XE 3817 black 9992 PA12
Cryogenic Tenelon High-Nitrogen Austenitic Stainless Steel, Annealed Bar, Plate, Sheet, Strip, UNS S21460
BASF Ultramid® B24 N 03 PA6

NSANDV5201 / 199765

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.