MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

RAMPF RAKU® TOOL IE-3461 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Low-Density Rigid Thixotropic; Rigid polyurethane

Key Properties:

  • Excellent physical properties after RT cure
  • Low density
  • Layup on vertical surfaces
  • Easy to sand
  • Easy to pigment
Applications:
  • For room temperature hand-batch processing
  • Ideal for theming masks, heads, and props
  • Prototype model making
  • Casting reproduction sculptures
Cure 1: 7 days at 77°F

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.680 g/cc0.0246 lb/in³Resin; ASTM D-792
 0.680 g/cc0.0246 lb/in³Hardener; ASTM D-792
 0.680 g/cc0.0246 lb/in³Cure 1; ASTM D-792
Viscosity 200 cP200 cPResin; ASTM D-2393
 1200 cP1200 cPHardener; ASTM D-2393
 2500 cP2500 cPMix; ASTM D-2393
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inCure 1; ASTM D-2566
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55 - 6555 - 65Cure 1; ASTM D-2240
Tensile Strength 16.5 MPa2400 psiCure 1; ASTM D-638
Elongation at Break 2.5 %2.5 %Cure 1; ASTM D-638
Flexural Strength 25.9 MPa3750 psiCure 1; ASTM D-790
Flexural Modulus 1.21 GPa175 ksiCure 1; ASTM D-790
Izod Impact, Notched 0.427 J/cm0.800 ft-lb/inCure 1; ASTM D-256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C140 °FCure 1; ASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 - 120 min1.00 - 2.00 hourMix, Demold time
Gel Time 4.00 - 6.00 min4.00 - 6.00 minMix
 
Descriptive Properties
AspectBeigeCure 1
Mix Ratio100:98Resin: Hardener, Weight
 100:98Resin: Hardener, Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAMPF042 / 317642

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.