Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product allowing to obtain optimum mechanical properties for form molding parts with a thickness over 10 mm. Information provided by NOVA Chemicals. |
Expanded Polystyrene, EPS |