MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
H.C. Starck FeCoCu Prealloyed Metal Powder
Categories: Metal; Ferrous Metal; Nonferrous Metal; Cobalt Alloy

Material Notes: A new prealloyed metallic powder of high sinter-activity with ideally homogenized constituents at an atomic level. The primary particles of very fine grain size are loosely agglomerated to agglomerate dimensions of around 30 micrometers. The powder can be used as cost effective alternative to pure cobalt powder and shows an excellent performance in professional stone cutting applications.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Bulk Density 0.700 g/ccScott Density; ASTM B329
 1.40 g/ccTap Density; ASTM B527
Particle Size 2.5 µmFisher sub sieve sizer; ASTM B330
Specific Surface Area 0.80 m²/gBET; ASTM D4567
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 99 - 116
 
Component Elements PropertiesOriginal ValueComments
Cobalt, Co 44 - 46 %
Copper, Cu 10 - 11 %
Iron, Fe 44 - 46 %
Oxygen, O <= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
H.C. Starck Amperit® 413.3 Gas Atomized (NiCoCrAlY)
H.C. Starck Grade HP Boron Carbide, B4C
H.C. Starck High Vacuum 120 Titanium Carbide, TiC
H.C. Starck Standard 250 Titanium Carbide, TiC
Overview of materials for Copper Alloy

NHCSTA062 / 17264

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.