MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Pyro-Bloc® T-Bar Module C Grade Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Pyro-Bloc T-Bar module is a ceramic fiber lining system designed for high temperature furnaces that often require corrosion barriers on the shell. The T-Bar module is manufactured from a high purity blend of raw materials which is used to produce C grade (alumina-silica-chromia).

Applications:

  • Process heaters
  • Heat transfer furnaces
  • Ethylene furnaces
  • Fume incinerators
  • All furnace linings requiring protective barrier against shell

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.192 g/cc
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0700 W/m-K
@Temperature 260 °C
at 192 kg/m3; ASTM C-201
 0.0700 W/m-K
@Temperature 260 °C
at 240 kg/m3; ASTM C-201
 0.120 W/m-K
@Temperature 538 °C
at 240 kg/m3; ASTM C-201
 0.140 W/m-K
@Temperature 538 °C
at 192 kg/m3; ASTM C-201
 0.210 W/m-K
@Temperature 816 °C
at 240 kg/m3; ASTM C-201
 0.240 W/m-K
@Temperature 816 °C
at 192 kg/m3; ASTM C-201
 0.320 W/m-K
@Temperature 1093 °C
at 240 kg/m3; ASTM C-201
 0.350 W/m-K
@Temperature 1093 °C
at 192 kg/m3; ASTM C-201
Melting Point 1760 °C
Maximum Service Temperature, Air <= 1371 °C
 <= 1427 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 43 %
Cr2O3 3.0 %
SiO2 54 %
 
Descriptive Properties
Colorblue/green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6472 / 203256

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.