MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epsan Eplamid 6 GFU 30 UV BK Q1D001 Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Polyamide 6, reinforced with 30% of glass fiber, heat stabilized, UV stabilizers and lubricated for injection molding. Eplamid 6 GFR 30 UV is used in all sectors of industry, offering a perfect balance of thermal and mechanical properties.

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inParallel; ISO 294-4
 0.0070 cm/cm0.0070 in/inNormal; ISO 294-4
Ash 30 %30 %ISO 3451-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress 100 MPa14500 psiConditioned; ISO 527-2
 160 MPa23200 psiDry; ISO 527-2
Elongation at Break 3.0 %3.0 %Dry; ISO 527-2
 6.0 %6.0 %Conditioned; ISO 527-2
Tensile Modulus 6.00 GPa870 ksiConditioned; ISO 527-2
 9.10 GPa1320 ksiDry; ISO 527-2
Flexural Strength 165 MPa23900 psiConditioned; ISO 178
 235 MPa34100 psiDry; ISO 178
Flexural Modulus 4.40 GPa638 ksiConditioned; ISO 178
 8.70 GPa1260 ksiDry; ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²5.71 ft-lb/in²Dry; ISO 180/1A
 15.0 kJ/m²7.14 ft-lb/in²Conditioned; ISO 180/1A
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²Dry; ISO 179/1eA
 1.60 J/cm²7.61 ft-lb/in²Conditioned; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75-2/A
Vicat Softening Point 210 °C410 °FISO 306/B50
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Dry; EN 60695-11-10
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Conditioned; EN 60695-11-10
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FRecommended Injection Molding Temperature
Drying Temperature 80.0 °C176 °FAverage Drying Time is 2-4 hrs
Moisture Content 0.20 %0.20 %ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epsan Eplamid 6 NC HV A3,6 Polyamide 6
Epsan Eplamid 66 GFI 20 NC Q1C0A801 Polyamide 66
Epsan Eplamid 6 FV2 NC Q1B801 Polyamide 6, Halogenated
Epsan Eplamid 6 FV0 NC Q1C001 Polyamide 6, Halogenated
Epsan Eplamid 6 CFR 30 BK Q1D001 Polyamide 6

PEPSAN043 / 186357

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.