MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ 303V-10 Polycarbonate Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Overview: CALIBRE™ 300V-10 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are available in 3 additive packages: CALIBRE 301V: Mold release. CALIBRE 302V: UV stabilizer. CALIBRE 303V: Mold release and UV stabilizer.

Govt. and Industry Standards:

  • CSA (Canadian Standards Association)
  • Underwriters Laboratory Inc. (UL)
Applications:
  • Electronic components
  • Lighting
  • Storage Media Housings

Information provided by Styron

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183/B; ASTM D792
Water Absorption 0.15 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62; ASTM D570
Moisture Absorption at Equilibrium 0.25 %
@Temperature 23.0 °C
50% RH; ISO 62; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 in/inISO 294-4; ASTM D955
Melt Flow 10 g/10 minASTM D1238
 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 71.0 MPaISO 527-2/50; ASTM D638
Tensile Strength, Yield 60.0 MPaISO 527-2/50; ASTM D638
Elongation at Break 150 %ISO 527-2/50; ASTM D638
Elongation at Yield 6.0 %ISO 527-2/50; ASTM D638
Tensile Modulus 2300 MPaISO 527-2/50
 2410 MPaASTM D638
Flexural Strength 96.5 MPaASTM D790
 97.0 MPa2.0 mm/min; ISO 178
Flexural Modulus 2400 MPa2.0 mm/min; ISO 178
 2410 MPaASTM D790
Izod Impact, Notched 910 J/m
@Temperature 23.0 °C
ISO 180/4A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
ASTM D256; ISO 180
Charpy Impact, Notched 35.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Dart Drop, Total Energy 87.0 JASTM D3763
Abrasion 45[%] Taber; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+17 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 60 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mmASTM D149
 17.0 kV/mmIEC 60243-1
Dissipation Factor 0.0010ASTM D150
Comparative Tracking Index 250 V
@Thickness 2.00 mm
Solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.0 µm/m-°CASTM D696
Hot Ball Pressure Test 125 °CIEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 141 °CAnnealed; ISO 75-2/B; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °CUnannealed; ISO 75-2/A
 125 °CUnannealed; ASTM D648
 138 °CAnnealed; ASTM D648
 143 °CAnnealed; ISO 75-2/A
Vicat Softening Point 146 °CISO 306/B50; ASTM D1525
Flammability, UL94 V-2
@Thickness 1.60 mm
 V-2
@Thickness 3.20 mm
Oxygen Index 26 %ISO 4289-2
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ASTM D542; ISO 489
Haze 1.0 %ASTM D1003
Transmission, Visible 89 %ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZZDWST040 / 142249

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.