Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as well as thermal shock protection.
Emerson & Cuming A-312 Stycast® One-Component General Purpose Encapsulant
- Excellent Chemical Resistance
- Unfilled
- Low viscosity
Cure Type: Heat Bonding Type: Epoxy The Stycast® product line is now a part of Henkel; this specific grade is discontinued. |