MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Latrobe DuraTech™ 20CV Powder Metal Stainless Tool Steel
Categories: Metal; Ferrous Metal; Stainless Steel; Tool Steel

Material Notes: DuraTech 20CV is a highly wear resistant, powder metallurgy stainless tool steel. The steel contains a large volume of extremely hard vanadium carbides, which provide excellent wear resistance. DuraTech 20CV contains the highest amount of chromium of any high-vanadium stainless steel currently available. The chromium-rich matrix provides outstanding corrosion resistance. DuraTech 20CV is a versatile stainless tool steel with a unique combination of high wear resistance, high corrosion resistance, good impact toughness, and excellent polishability. This combination of properties is the result of the fine grain size, small carbides, and superior cleanliness of the powder metallurgy (PM) microstructure. DuraTech 20CV excels in applications, which require a combination of high wear resistance. The unique combinations of properties makes DuraTech 20CV an excellent steel for plastic injection feed screws, barrel liners, screw tips, and mold cavities, especially for plastic resins which contain abrasive fill

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.275 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 54Oil Quenched from 1071°C; 540°C Temper Temperature
 59Oil Quenched from 1071°C; 410°C Temper Temperature
 60Oil Quenched from 1071°C; As Quenched
Modulus of Elasticity 31000 ksi
Machinability 35 - 40 %1% Carbon Steel
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.9 µm/m-°C
@Temperature 20.0 - 100 °C
 12.3 µm/m-°C
@Temperature 20.0 - 500 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.9 %
Chromium, Cr 20 %
Iron, Fe 71.9 %
Manganese, Mn 0.30 %
Molybdenum, Mo 1.0 %
Silicon, Si 0.30 %
Tungsten, W 0.60 %
Vanadium, V 4.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel
AISI Type P20 Mold Steel (UNS T51620)
AISI Type P2 Mold Steel (UNS T51602)
AISI Type P4 Mold Steel, air cooled from 955°C, tempered at 425°C
AISI Type P3 Low carbon Mold Steel (UNS T51603)

NTIMK129 / 19476

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.