MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
International Mold Steel S-Star 420 ESR Stainless Steel for Plastic Molds
Categories: Metal; Ferrous Metal; Stainless Steel; Tool Steel; Mold Steel

Material Notes: Characteristics:
  • Excellent corrosion resistance
  • High hardness; up to 53 HRC
  • Superb mirror-finish surface
  • Minimal distortion, less than 0.03% after heat treatment
  • Excellent internal matrix by ESR
  • Uniform texture surface by photo etching and electrical discharge machining

Applications:
  • Ultra mirror finish plastic molds - Lens
  • Ultra-hard, Corrosion-resistance plastic molds - Medical Instruments, Cosmetic containers, Food containers
  • Example Resins: PMMA, PC, PP, PS, PVC, PE, PF, Flame resisting compounds

Information provided by International Mold Steel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.70 g/cc
@Temperature 400 °C
 7.73 g/cc
@Temperature 300 °C
 7.75 g/cc
@Temperature 200 °C
 7.78 g/cc
@Temperature 100 °C
 7.80 g/cc
@Temperature 20.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 32Pre-Hardened
 53Heat Treated
Tensile Strength, Ultimate 1100 MPaPre-Hardened
 1940 MPaHeat Treated
Tensile Strength, Yield 890 MPa
@Strain 0.2 %
Pre-Hardened
 1540 MPa
@Strain 0.2 %
Heat Treated
Elongation at Break 9.0 %Heat Treated
 15 %Pre-Hardened
Reduction of Area 28 %Heat Treated
 55 %Pre-Hardened
Modulus of Elasticity 190 GPa
@Temperature 400 °C
Longitudinal
 200 GPa
@Temperature 300 °C
Longitudinal
 209 GPa
@Temperature 200 °C
Longitudinal
 212.5 GPa
@Temperature 100 °C
Longitudinal
 214.5 GPa
@Temperature 20.0 °C
Longitudinal
Charpy Impact Unnotched 25.0 J/cm²Heat Treated; 2uE
 60.0 J/cm²Pre-Hardened; 2uE
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.8 µm/m-°C
@Temperature 20.0 - 100 °C
 11.1 µm/m-°C
@Temperature 20.0 - 200 °C
 11.3 µm/m-°C
@Temperature 20.0 - 300 °C
 11.5 µm/m-°C
@Temperature 20.0 - 400 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 23.0 W/m-K
@Temperature 20.0 °C
 23.4 W/m-K
@Temperature 100 °C
 23.9 W/m-K
@Temperature 200 °C
 24.7 W/m-K
@Temperature 300 °C
 25.1 W/m-K
@Temperature 400 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.38 %
Chromium, Cr 13.5 %
Iron, Fe 84.8 %As Remainder
Molybdenum, Mo 0.1 %
Silicon, Si 0.9 %
Vanadium, V 0.3 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EDRO RoyAlloy™ #6 Free Machining Stainless Holder Steel
Bohler-Uddeholm UDDEHOLM STAVAX® ESR Modified 420
440C Martensitic Stainless Steel (UNS S44004)
420 Stainless Steel, hardened and tempered bar
AK Steel 420 Martensitic Stainless steel

NIMSA00 / 217529

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.