MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Taiwan PU CPU-107-317A-A/B Hybrid PU Spray Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Key features:
  • Hardness: 70A, 90A
  • Mixing ratio: 1:1 by volume
  • 100% solid content
  • Fast reactivity
  • Good mechanical property
  • Wide range of application
Description: Hybrid PU spray coating CPU-107-309A-A/B, CPU-107-317A-A/B and CPU-107-319A-A/B are solvent free two component hybrid based material for waterproofing membrane with high resistance to many chemicals, anti-corrosion and anti-abrasion.

Characteristics:

  • 1. Fast reacting
  • 2. Solvent free
  • 3. Seamless
  • 4. Crack bridging capacity
  • 5. Elastomeric at low temperature
  • 6. High mechanical properties

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 - 1.06 g/cc1.00 - 1.06 g/ccPart A
 1.05 - 1.11 g/cc1.05 - 1.11 g/ccPart B
Solids Content 100 %100 %
Viscosity 270 - 470 cP270 - 470 cPPart B
 350 - 550 cP350 - 550 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070
Tensile Strength >= 10.0 MPa>= 1450 psi
Elongation at Break >= 590 %>= 590 %
Tear Strength >= 49.0 kN/m>= 280 pli
 
Processing PropertiesMetricEnglishComments
Cure Time 0.333 - 0.667 min0.00556 - 0.0111 hourTack free time
Gel Time 11.0 - 12.0 min11.0 - 12.0 min
Shelf Life 12.0 Month
@Temperature 20.0 - 30.0 °C
12.0 Month
@Temperature 68.0 - 86.0 °F
 
Descriptive Properties
AppearanceLight yellowPart B
 Viscous liquidPart A
Mixing ratio100:100by volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTAIWPU039 / 305769

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.