MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Zoltek™ PX35 P/TW28-50 Woven Carbon Fiber Fabric
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: ZOLTEK PX35 Tow Weave Carbon Fabrics are produced from ZOLTEK PX35 50K Continuous Tow Carbon Fiber. Quick composite part build-up is cost effectively achieved with cosmetically attractive carbon fiber fabrics. Applications include large composite tooling parts and aesthetically appealing finished composite components.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.81 g/cc
Thickness 1500 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 4137 MPaContinuous Tow
Elongation at Break 1.5 %Continuous Tow
Tensile Modulus 242 GPaContinuous Tow
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00155 ohm-cm
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 95 %
 
Descriptive Properties
Areal Weight960 g/m2
ConstructionPlain or twill weave.
Fiber Diameter (µm)7.2
Fill Yarn1.5/cm
Roll Length30 m
Roll Width1.27 m
Warp Yarn1/cm
YarnZoltek PX35 50K tow with Epoxy sizing at 1.5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zoltek™ PX35 SW48-50 Woven Carbon Fiber Fabric
Zoltek™ PX35 Continuous Tow Carbon Fiber
Solvay CYCOM® 5250-4 BMI Prepreg System with AS4-3K-70PW Woven Carbon Fiber
Zoltek™ PX35 UD150 Uni-Directional Carbon Fabric
DowAksa AKSACA™ A-38 3K Continuous Carbon Fiber

ECZO812 / 232280

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.