MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chemical Concepts Chem-Set™ 735 High Performance Hot Melt Adhesive
Categories: Polymer; Adhesive; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: A amber high strength hot melt adhesive perfect for coated cardboard. This hot melt adhesive has a medium set time, and a very hot tack. Its high strength makes it perfect for coated paper or cardboard. Applications: Packaging, Product assembly, woodworking and furniture. Bonds: Ceramic, wood, cardboard, plastic, general purpose.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Brookfield Viscosity  3475 cP
@Temperature 375 °C
3475 cP
@Temperature 707 °F
spindle SC4-27; ASTM D3236
 7350 cP
@Temperature 325 °C
7350 cP
@Temperature 617 °F
spindle SC4-27; ASTM D3236
 31250 cP
@Temperature 250 °C
31250 cP
@Temperature 482 °F
spindle SC4-27; ASTM D3236
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 50.6 °C123 °FPeel Adhesion Failure. ASTM D4498, 45# Kraft paper substrates, 100 g weights.
Flash Point >= 232 °C>= 450 °F
Shear Adhesion Failure Temperature 75.0 °C167 °F45# Kraft paper substrates, 500 g weights; ASTM D4498
 
Processing PropertiesMetricEnglishComments
Processing Temperature 163 - 193 °C325 - 380 °FApplication
 
Descriptive Properties
Chemical CompositionEthylene Vinyl Acetate
ColorAmber clear
Mettler Softening Point185°F, ASTM D6493-99
Odorslight
Open Time25 sec. ASTM D4497-94(1999) using 45# Kraft paper substrates

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Northern White Pine Wood
Solvay BR® 127 Corrosion Inhibiting Epoxy Primer
Overview of materials for Thermoset Polyurethane Foam, Glass Filled
Dow 722 Low Density Polyethylene (LDPE)

PCHEMI927 / 232186

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.