MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
A. Schulman Premi-Glas® 2200-22 Fiberglass Reinforced SMC  (discontinued **)
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: Description: Premi-Glas® 2200-22 is a fiberglass reinforced thermoset Sheet Molding Compound similar to the Premi-Glas® 2200-22 CR-SX product. Unlike the -CR-SX version, this product carries no UL recognition.

Key features and benefits:

  • Level of flame retardance may vary by specific formula to meet customer needs
  • Greater formulating latitude to meet special molding characteristics or end properties
  • Not subject to any Underwriters Laboratories testing or follow-up

Market: Electrical/Flame Retardant

Information provided by Premix.

A. Schulman has acquired this former Premix product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Linear Mold Shrinkage 0.0015 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 8000 psiASTM D638
Tensile Modulus 1.50e+6 psitangent; ASTM D638
Flexural Strength 20000 psiASTM D790-1
Flexural Modulus 1.30e+6 psiTangent; ASTM D790-1
Poissons Ratio 0.30ISO 527
Izod Impact, Notched 13.0 ft-lb/inASTM D256
Izod Impact, Unnotched 17.0 ft-lb/inASTM D4812
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 380 V/milASTM D149
Comparative Tracking Index 600 VASTM D2303
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µin/in-°F
@Temperature 20.0 °C
Z-direction; ASTM D696
CTE, linear, Transverse to Flow 15.0 µin/in-°F
@Temperature 20.0 °C
XY-direction; ASTM D696
Specific Heat Capacity 0.360 BTU/lb-°FASTM D1269E
Thermal Conductivity 2.08 BTU-in/hr-ft²-°FASTM D1269E

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Premi-Glas® 1200-30 Polyester SMC
Haysite 46000 Polyester SMC, 30% Glass Reinforced
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP
Menzolit Menzolit® SMC 0600 Unsaturated Polyester UP
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP

PPREMI14 / 58141

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.