MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

ITW Devcon® Titanium Putty
Categories: Polymer; Thermoset; Epoxy

Material Notes: High-tech, titanium-reinforced epoxy putty engineered for making critical repairs to machinery and precision parts. Use; Restore bearing housings and scored shafts; rebuild wear rings, hydraulic rams, and valves; repair equipment and parts that require a machined finish. Features: High compressive strength Temperature resistance to 350°F Resistant to chemicals and most acids, bases, solvents, and alkalis.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.36 g/cc2.36 g/cc
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8787ASTM D2240
Modulus of Elasticity 6.55 GPa950 ksi
Flexural Strength 53.1 MPa7700 psiASTM D790
Compressive Strength 105 MPa15200 psiASTM D695
Shear Strength 13.8 MPa2000 psiASTM D1002
Adhesive Bond Strength 13.8 MPa2000 psiAdhesive Tensile Shear; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 44.844.8ASTM D150
Dielectric Strength 2.20 kV/mm55.9 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 39.6 µm/m-°C22.0 µin/in-°FASTM D696
Thermal Conductivity 0.816 W/m-K5.66 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 65.6 °C150 °FTemperature Resistance - Wet
 177 °C350 °FTemperature Resistance - Dry
Shrinkage 0.10 %0.10 %Linear During cure; ASTM D2566
 
Processing PropertiesMetricEnglishComments
Cure Time  960 min
@Temperature 24.0 °C
16.0 hour
@Temperature 75.2 °F
Functional cure
 10100 min
@Temperature 24.0 °C
168 hour
@Temperature 75.2 °F
As Tested
Pot Life 21.0 min
@Temperature 23.9 °C
21.0 min
@Temperature 75.0 °F
 
Descriptive Properties
Chemical/Solvent ResistanceAcetic (diluted) 10%: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Benzene: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Gasoline (Unleaded): Excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Kerosene: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Mineral Spirits: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Nitric 50%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Phosphoric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Potassium Hydroxide 40%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 50%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hypochlorite: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric 50%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Toluene: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Trisodium Phosphate: excellent30 day immersion at 75°F. Sample cured 7 days at RT
ColorGray
Coverage47 ft²Cured. @ 1/4"
Mix Ratio by volume3.1:1
Mix Ratio by weight4.3:1
Recoat Time7 hrs
Specific Volume (in.³/lb)11.7Cured
ViscosityMixed. Putty

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWD9195 / 239705

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.