Hostacom EBG 2145T BLACK is a 20% glass fiber reinforced PP (coupled). It is designed for applications requiring a high level of long term heat ageing. The use of the new "Advanced Copo PP" resin provides a significantly higher mechanical durability under load at elevated temperatures due to much lower material deformation (creep) compared to existing PP Compounds. The product is available as black colored, pellet form. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Automotive Parts Market: Automotive Processing Method: Injection Molding Information provided by LyondellBasell. |