MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
China Tungsten YWC Tungsten Carbide for Dies and Wear Part Making
Categories: Ceramic; Carbide

Material Notes: Magnetic conductivity non-magnetic alloy with very high strength ,excellent  wear resistance and very low magnetic conductivity . used for forming die for permanent-magnetic materials with a high service endurance up to 0.5~1M times

Information provided by China Tungsten

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell A >= 87.5
Flexural Strength 1700 MPa
 
Electrical PropertiesOriginal ValueComments
Magnetic Permeability <= 1.0005

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ICE Hot Pressed SiC
H.C. Starck Amperit® 599.074 Agglomerated Sintered Molybdenum Carbide (Cr2O3)
H.C. Starck Amperit® 582.072 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr)
Goodfellow Tungsten 95/Titanium 5 Alloy
Diamond, Polycrystalline

NCHIN093 / 78935

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.