MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aleris Alustar Aluminum Alloy, H321/H116; 20 - 40 mm thickness
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: At least 20% stronger than AA 5083 before and after welding. Bendability and weldability similar to AA 5083. High corrosion resistance. Provides options for ship design and building.

Composition differs from standard 5083 and 5383 mainly in terms of higher Mg-content, higher Mn-content, higher Zn-content, and defined Zr-content. The increased Mg-content in the Alustar alloy increases the strength after welding. Together with an increased Mn-content, a higher Mg-content enhances the ductility. To compensate for the deterioration in corrosion resistance caused by the higher Mg-content, an optimal amount of Zn is required. By precipitating Mg-Zn-containing phases in the Al matrix, potential differences between the grain boundaries and grain interiors are eliminated. Zr additions to Alustar alloy cause the formation of a finer grained heat affected zone which leads to a stronger bond in the fusion zone. The effect of Zr is the same in welding wires. Therefore, in addition to the standard filler alloys such as AA5183, Zr-containing filler wires (such as AA 5087) can also be used to weld Alustar alloy plates.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.66 g/cc0.0961 lb/in³Aluminum 5083
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 360 MPa>= 52200 psi
Tensile Strength, Yield >= 260 MPa>= 37700 psi
Elongation at Break 10 %10 %
Shear Strength 215 MPa31200 psiCalculated
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 93 %93 %
Chromium, Cr <= 0.30 %<= 0.30 %
Copper, Cu <= 0.40 %<= 0.40 %
Iron, Fe <= 0.50 %<= 0.50 %
Magnesium, Mg 5.0 - 6.0 %5.0 - 6.0 %
Manganese, Mn 0.60 - 1.2 %0.60 - 1.2 %
Silicon, Si <= 0.50 %<= 0.50 %
Titanium, Ti <= 0.20 %<= 0.20 %
Zinc, Zn 0.40 - 1.5 %0.40 - 1.5 %
Zirconium, Zr 0.050 - 0.25 %0.050 - 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aleris Alustar Aluminum Alloy, H321/H116; 2 - 20 mm thickness
Aluminum 7039-T61
Aluminum 5083-H116; 5083-H321
5059 Aluminum Composition Spec
Aluminum 5383-H321/H116

NHOOG01 / 17341

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.