MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF Ultramid® T KR 4365 G5 Nylon 6/6T, 25% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Ultramid T KR 4365 G5 is a 25% glass fiber reinforced, flame-retardant, injection molding PA6/6T grade. Good mechanical properties, high tracking resistance, low tendency for deposits on electrical contacts, very resistant to electrolytic corrosion, resistant to solder baths; electroplateable. Flame retardant based on red phosphorus.

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ISO 1183
Moisture Absorption 1.30 %1.30 %50% RH; ISO 62
Water Absorption at Saturation 5.5 %5.5 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  96.0 MPa
@Temperature 80.0 °C
13900 psi
@Temperature 176 °F
Dry; ISO 527
 140 MPa
@Temperature 23.0 °C
20300 psi
@Temperature 73.4 °F
Conditioned; ISO 527
 150 MPa
@Temperature 23.0 °C
21800 psi
@Temperature 73.4 °F
Dry; ISO 527
 177 MPa
@Temperature -40.0 °C
25700 psi
@Temperature -40.0 °F
Conditioned; ISO 527
 192 MPa
@Temperature -40.0 °C
27800 psi
@Temperature -40.0 °F
Dry; ISO 527
Elongation at Break  2.5 %
@Temperature 80.0 °C
2.5 %
@Temperature 176 °F
Dry; ISO 527
 2.6 %
@Temperature -40.0 °C
2.6 %
@Temperature -40.0 °F
Conditioned; ISO 527
 2.9 %
@Temperature -40.0 °C
2.9 %
@Temperature -40.0 °F
Dry; ISO 527
 3.0 %
@Temperature 23.0 °C
3.0 %
@Temperature 73.4 °F
Dry; ISO 527
 3.0 %
@Temperature 23.0 °C
3.0 %
@Temperature 73.4 °F
Conditioned; ISO 527
Tensile Modulus 8.00 GPa1160 ksiConditioned; ISO 527
 8.30 GPa1200 ksiDry; ISO 527
Charpy Impact Unnotched  7.50 J/cm²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179
 8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmDry; IEC 60093
Dielectric Constant 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
Dry; IEC 60250
Dissipation Factor 0.20
@Frequency 1e+6 Hz
0.20
@Frequency 1e+6 Hz
Dry; IEC 60250
Comparative Tracking Index 600 V600 VConditioned; IEC 60112
 600 V600 VDry; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C13.9 µin/in-°F
CTE, linear, Transverse to Flow 55.0 µm/m-°C30.6 µin/in-°F
Melting Point 295 °C563 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FISO 75
UL RTI, Electrical  140 °C
@Thickness 0.750 mm
284 °F
@Thickness 0.0295 in
UL746B
 140 °C
@Thickness 1.50 mm
284 °F
@Thickness 0.0591 in
UL746B
 140 °C
@Thickness 3.00 mm
284 °F
@Thickness 0.118 in
UL746B
UL RTI, Mechanical with Impact  100 °C
@Thickness 0.750 mm
212 °F
@Thickness 0.0295 in
UL746B
 105 °C
@Thickness 1.50 mm
221 °F
@Thickness 0.0591 in
UL746B
 110 °C
@Thickness 3.00 mm
230 °F
@Thickness 0.118 in
UL746B
UL RTI, Mechanical without Impact  120 °C
@Thickness 0.750 mm
248 °F
@Thickness 0.0295 in
UL746B
 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL746B
 140 °C
@Thickness 3.00 mm
284 °F
@Thickness 0.118 in
UL746B
Flammability, UL94  V-2
@Thickness 0.370 mm
V-2
@Thickness 0.0146 in
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 5VA
@Thickness 1.50 mm
5VA
@Thickness 0.0591 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF8985 / 254943

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.