MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Momentive Performance Materials TUFEL™ III 92506 Biocompatible Extrusion Heat Cured Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance standards.

TUFEL III Biocompatible Extrusion 92506 is a member of the Addition Curing Portfolio. It is a platinum (addition/heat) curable, one-part compound. This product has been optimized for extrusion and calendering processes and is intended for application in the Healthcare industry.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050
Tensile Strength 7.60 MPa1100 psi
Elongation at Break 500 %500 %
Tear Strength 18.0 kN/m103 pliDie B
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 20 %20 %translucent; thickness unknown
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFDA Indirect food contact - Rubber articles intended for repeated use - FDA Reg 21CFR177.2600
USP Class VI YesYesUSP Class VI methods: Intramuscular implantation, intracutaneous injection, & systematic injection
 
Descriptive Properties
AppearanceTranslucent
ISO10993yes7 ISO 10993 tests applicable to "wet" chemicals

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP46HT-2Med Two Component Heat Resistant Biocompatible Epoxy System
CPT C-Flex® R70-190 Opaque Biocompatible TPE
Americhem Engineered Compounds ColorRx™ PP2-1002ARX Biocompatible Polypropylene Random Copolymer
Americhem Engineered Compounds ColorRx™ PP1-2000RX Biocompatible Polypropylene Homopolymer
Americhem Engineered Compounds ColorRx™ PE3-0200RX Biocompatible LDPE

PGE8V833 / 109093

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.