MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
BryCoat Thermal Spray Coatings
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Thermal spray coatings are applied by spraying fine powdered materials to the part surface at extremely high velocities. The resulting coatings can be from 0.0005 inches to over 0.100 inches. Thermal spray coatings are used for
  • Wear Resistance
  • Corrosion Resistance
  • Abrasion Resistance
  • Dimensional Restoration
  • Thermal Barrier
Many different coating materials can be used, such as ceramics, MCrAlYs, carbides, oxides, and alloys. Coating systems include HVOF (High Velocity Oxy Fuel) and High Energy Air Plasma.

Attributes of plasma spray coating:

  • Cost Effective
  • Good Wear Factor
  • Bond Tensile Strength (6000 psi typical)
  • High Density (15% porosity)
  • Excellent for Thermal Barrier Coatings (TBCs)
Attributes of HVOF Coating:
  • Excellent Wear Factor
  • Very High Density (1% porosity)
  • Outstanding Adhesion
  • Bond Tensile Strength (15,000 psi typical)

Information provided by BryCoat, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Specialty Coating Systems Parylene C Poly (P-Xylylene) Coating
Titanium Nitride (TiN) Coating
Titanium Aluminum Nitride (TiAlN) PVD Coating
Tantalum Carbide, TaC
Molybdenum Carbide, Mo2C

NTHERMSP / 19276

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.