MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

American Elements Silicon Oxide Nanopowder
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: General Description

Silicon Oxide (SiO2) Nanopowder, Silica Nanoparticles or nanodots are high surface area particles. Nanoscale Silicon Oxide Nanoparticles or Silica Particles are typically 5 - 100 nanometers (nm) with specific surface area (SSA) in the 25 – 50 m 2 /g range. Nano Silicon Oxide Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Research into applications for Silicon Oxide nanocrystals includes use as a dielectric coating, in solar cell applications, as a high temperature insulator, as a gas sensor and for use in other coatings, plastics, polymers and wire and further research for their potential electrical, optical, imaging, and other properties Silicon Oxide Nano Particles are generally immediately available in most volumes.

Key Words: Formula: SiO2; CAS Number: 60676-86-0
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.533 g/cc0.09151 lb/in³
Particle Size 0.0050 - 0.10 µm0.0050 - 0.10 µm
Specific Surface Area 25 - 50 m²/g25 - 50 m²/g
Molecular Weight 60.09 g/mol60.09 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 1710 °C3110 °F
Boiling Point 2590 °C4690 °F
 
Descriptive Properties
AppearanceWhite Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silicon Dioxide, SiO2 (Alpha Quartz)
Quartz (SiO2)
Silicon Dioxide, SiO2 (Coesite)
Borosilicate Glass, Low Expansion
Borosilicate Glass

EJAMER77 / 5560

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.