MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

(Viewing data as-entered. Click here to return)
Multibase C6-250 PERKADOX PD-50S Dow-Corning Class VI Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes:

Information provided by Multibase

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccRelative, molded-without post cure; ASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 44molded- without post cure; ASTM D2240
 46post cured- 4 hours at 177°C; ASTM D2240
 49post cured- 2 hours at 177°C; ASTM D2240
 50post cured- 8 hours at 177°C; ASTM D2240
Tensile Strength, Ultimate 1200 psimolded-without post cure; ASTM D412
 1200 psipost cured- 2 hours at 177°C; ASTM D412
 1300 psipost cured- 8 hours at 177°C; ASTM D412
 1400 psipost cured- 4 hours at 177°C; ASTM D412
Tensile Strength, Yield 330 psiat 200%, molded-without post cure; ASTM D412
 370 psiat 200%, post cured- 2 hours at 177°C; ASTM D412
 390 psi200%, post cured- 4 hours at 177°C; ASTM D412
 390 psi200%, post cured- 8 hours at 177°C; ASTM D412
Elongation at Break 530 %post cured- 2 hours at 177°C; ASTM D412
 530 %post cured- 8 hours at 177°C; ASTM D412
 550 %post cured- 4 hours at 177°C; ASTM D412
 560 %molded-without post cure; ASTM D412
Tear Strength 140 pliDie B, post cured- 8 hours at 177°C; ASTM D624
 150 pliDie B,molded-without post cure; ASTM D624
 150 pliDie B, post cured- 2 hours at 177°C; ASTM D624
 150 pliDie B, post cured- 4 hours at 177°C; ASTM D624
Compression Set 61 %
@Temperature 177 °C,
Time 79200 sec
post cured- 4 hours at 177°C; ASTM D395
 63 %
@Temperature 177 °C,
Time 79200 sec
post cured- 2 hours at 177°C; ASTM D395
 73 %
@Temperature 177 °C,
Time 79200 sec
post cured- 8 hours at 177°C; ASTM D395
 96 %
@Temperature 177 °C,
Time 79200 sec
molded-without post cure; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Shrinkage 2.0 %
@Temperature 177 °C,
Time 7200 sec
post cured
 2.2 %
@Temperature 177 °C,
Time 14400 sec
post cured
 2.3 %
@Temperature 177 °C,
Time 28800 sec
post cured
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NuSil MED-2174 One-Part Standard High Consistency Elastomer - Unrestricted Medical Use
Westlake EM1550AA Low Density Polyethylene
IDI Composites Dielectrite® 48-50 Thermoset Polyester, Molding
Palladium, Pd
Westlake Plastics Dielux® PTFE filled Acetal Copolymer

PMULTI159 / 54063

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.