MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Terves TAx-100E Frac Ball
Categories: Metal

Material Notes: TervAlloyFracBalls are created from our patent-pendingTAx-100E™, TAx-50E™, and Z-1000C alloys, and have become recognized as the industry standard for consistent performance and value. Available in both stock and custom sizes, these high performance fracballs will dissolve in potassium chloride and sodium chloride solutions. TervAlloyFracBalls can also be provided with various Response Coatings™ applied to modify or extend particular dissolution rates. General guidelines for TervAlloyFracBalls are as follows:
  • Twenty-eight standard sizes, though any size may be specified up to 4.95 in.
  • Standard tolerances are +.000,-.003 (tighter tolerances may be available upon request)
  • KCl/brine, acid, and freshwater alloys are available

Information provided by Terves Incorporated

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 40.0 ksi
Tensile Strength, Yield 26.5 ksi
Elongation at Break 8.8 %
 
Descriptive Properties
Dissolution rate32at 90° C (mg/cm²•hr) - 3%KCl
Dissolves inKCl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTERVES000 / 314468

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.