MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ganpati Exim 1705 (SKMS-30 ARKM-15) SBR
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Butadine - Styrene synthetic rubbers are produced via emulsion copolymerization of butadiene and styrene. These rubbers do not require special mastification. Hey are good miscible with different ingredients of rubber mixtures and are good compatible with another general purpose rubber tires (BR, polyisoprene).

Application: The SBR1705 is general purpose rubber. Used in tire industry for tire treads and another tire parts, in rubber technical and footwear industries for production of white and color rubber shoes. It is mainly used for adhesives, sealant etc and a lot of rubber products including tires, shoes, rubber hose, belting etc.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 45 - 54
@Temperature 100 °C
ML (1+4)
Ash <= 0.80 %
 
Chemical PropertiesOriginal ValueComments
Styrene Content 21 - 24 %A-metylstyrene or metylmethactrylate
 22 - 25 %Bounder monomer
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength <= 24.5 MPa
Elongation at Break 550 - 750 %
Rebound <= 27 %Elasticity
 
Descriptive Properties
Content<0.3%Mass Fraction of Organic Acids Soaps
 0.15-0.35%Mass fraction of antioxidant VS-1
 0.6-1.2%Mass fraction of antioxidant Agidol-2
 0.6-1.2%Mass fraction of antioxidant P-23 (alkofen B)
 1.0-1.5%Mass fraction of antioxidant VTS-150
 1.0-2.0%Mass fraction of antioxidant VS-30 A
 14-17%Mass Fraction of Oil
 5-6.7%Mass Fraction of Organic Acids
Mass losses at drying<0.4%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGANPATI022 / 317306

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.