MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polymer Resources ABS-GP-HH General Purpose ABS, High Heat
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes: General Purpose Acrylonitrile Butadiene Styrene, High Heat

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 1.0 - 5.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
1.0 - 5.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 112112ASTM D785
Tensile Strength at Break 42.1 MPa6100 psiASTM D638
Tensile Strength, Yield 44.8 MPa6500 psiASTM D638
Elongation at Break 25 %25 %ASTM D638
Elongation at Yield 4.5 %4.5 %ASTM D638
Tensile Modulus 2.21 GPa320 ksiASTM D638
Flexural Strength 79.3 MPa11500 psiASTM D790
Flexural Modulus 2.48 GPa360 ksiASTM D790
Izod Impact, Notched  0.534 J/cm
@Temperature -40.0 °C
1.00 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 1.87 J/cm
@Temperature 22.8 °C
3.50 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Izod Impact, Notched (ISO)  6.30 kJ/m²
@Temperature -30.0 °C
3.00 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 13.0 kJ/m²
@Temperature 22.8 °C
6.20 ft-lb/in²
@Temperature 73.0 °F
ISO 180/1A
Charpy Impact, Notched 1.05 J/cm²
@Temperature 22.8 °C
5.00 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eA
Gardner Impact 22.6 J16.7 ft-lbASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C215 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.6 °C195 °FASTM D648
Vicat Softening Point 116 °C240 °F120°C/h, 50 N; ASTM D1525
Flammability, UL94  HB
@Thickness 1.59 mm
HB
@Thickness 0.0626 in
 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 193 - 210 °C380 - 410 °F
Middle Barrel Temperature 216 - 238 °C420 - 460 °F
Front Barrel Temperature 227 - 254 °C440 - 490 °F
Melt Temperature 232 - 274 °C450 - 525 °F
Mold Temperature 48.9 - 82.2 °C120 - 180 °F
Drying Temperature 82.2 - 93.9 °C180 - 201 °F
Dry Time 2.00 - 5.00 hour2.00 - 5.00 hour
Vent Depth 0.00254 cm0.00100 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TPI Porene® ABS-KU650 Super High Heat ABS Resin
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Omni Plastics OmniTech™ ABS 24 HH ABS
LG Chemical XR-472 ABS, High Heat Resistance, High Gloss

PPOLYQ012 / 160525

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.