MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Materion BrushForm® 158 Strip Copper-Nickel-Tin, TM19 (UNS C72900)
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: BrushForm® 158 strip is a high-performance, heat treated spinodal copper-nickel-tin alloy designed to provide optimal photochemical machinability, high yield strength and increased fatigue life. The TM18 and TM19 tempers provide excellent flatness and stiffness coupled with high resistance to vibration, fatigue, and impact loading. This makes them ideal for voice coil motor springs in optical image stabilization systems.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.00 g/cc0.325 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers >= 375>= 375
Tensile Strength, Ultimate 1410 MPa205000 psi
Tensile Strength, Yield 1375 MPa
@Strain 0.200 %
199400 psi
@Strain 0.200 %
Elongation at Break 1.40 %1.40 %
Modulus of Elasticity 119 - 145 GPa17300 - 21000 ksi
Poissons Ratio 0.3000.300
Shear Modulus 45.8 - 55.8 GPa6640 - 8090 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000250 ohm-cm0.0000250 ohm-cm
Magnetic Permeability <= 1.01<= 1.01
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.4 µm/m-°C9.11 µin/in-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 76.0 - 78.0 %76.0 - 78.0 %
Nickel, Ni 14.5 - 15.5 %14.5 - 15.5 %
Tin, Sn 7.50 - 8.50 %7.50 - 8.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NBB63437d / 323498

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.