MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Brandenburger BRA_GLA N Thermal Insulation Board
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset

Material Notes: A material with high quality glass fibre fabric and roving layers in conjunction with heat resistant EP matrix, which provides a thermal protection with excellent compressive and flexural strength, as well as high interlaminar shear strength. Suited for applications such as injection moulds, packing machines, frame and piston insulations in wood processing presses.

Information provided by Brandenburger Isoliertechnik GmbH&Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.00 g/cc0.0723 lb/in³
Water Absorption 0.20 %0.20 %24 hrs; DIN 53 495
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 550 MPa79800 psiEN 63
 180 MPa
@Temperature 200 °C
26100 psi
@Temperature 392 °F
EN 63
Flexural Modulus 27.0 GPa3920 ksiEN 63
 20.5 GPa
@Temperature 200 °C
2970 ksi
@Temperature 392 °F
EN 63
Compressive Strength 600 MPa87000 psiEN ISO 604
 290 MPa
@Temperature 200 °C
42100 psi
@Temperature 392 °F
EN ISO 604
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 µm/m-°C
@Temperature 20.0 °C
5.56 µin/in-°F
@Temperature 68.0 °F
DIN 53752
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°FDIN 52 612
Maximum Service Temperature, Air 210 °C410 °FLong Term
 230 °C446 °FShort Term

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Brandenburger S 4000 HT Thermal Insulation Board
Brandenburger S 2000 A Side Insulation
Brandenburger KV 3 Thermal Insulation Board
Brandenburger ISOFLEX AFV Foam
Brandenburger Heavy Duty Mounting Paste

PBRAND01 / 27712

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.