MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NuSil MED-6020 Silicone, Low Consistency Elastomer - Restricted Medical Use
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: Low consistency elastomers (LCEs) are useful alternatives to liquid silicone rubber (LSR) and high consistency rubber (HCR) for end users who need a low viscosity elastomer which provides other unique properties.

Important Properties: LCEs lend themselves to applications that require a pourable, selfleveling silicone. Applications include: encapsulating a device, backfilling a void, potting an electronic component that cannot withstand exposure to high heat, or prototyping a mold. Features of low consistency elastomers may include the following:

  • Optically clear
  • Self-leveling
  • Low and high temperature cure
  • Low viscosity
  • Easy to process
Comments: Optically Clear

Cure System: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
Viscosity 40000 cP40000 cPB
 70000 cP70000 cPA
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040Typical
 35 - 4535 - 45Certified
Tensile Strength at Break 3.50 MPa508 psiCertified
 4.40 MPa638 psiTypical
Elongation at Break 100 %100 %Certified
 175 %175 %Typical
Tear Strength 4.38 kN/m25.0 pliCertified
 6.14 kN/m35.0 pliTypical
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min
@Temperature 150 °C
0.500 hour
@Temperature 302 °F
Working Life 240 min
@Temperature 25.0 °C
240 min
@Temperature 77.0 °F
 
Descriptive Properties
Mix Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNUSIL435 / 142159

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.