Kaowool HT is a low cost high temperature product designed for use up to 2600°F (1427°C). Kaowool HT is a rigid self-supporting product produced in a variety of sizes and thicknesses. Applications: Appliance and heat processing Backup insulation to dense refractories Bullnose tiles Burner blocks Combustion chamber construction Expansion joint material Flue and chimney linings Furnace components Furnace door linings Furnace, kiln, and oven hot face linings Glass regenerator insulation Heat shields High temperature gaskets and seals Peep door frames and plugs Shapes in ammonia reformersInformation provided by Thermal Ceramics Data has not been recently verified. Please contact manufacturer for current information. |