MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Elvaloy® 4170 Reactive Ethylene Terpolymer (RET)
Categories: Polymer; Thermoplastic

Material Notes: A reactive ethylene terpolymer (RET) that can be used to modify the properties of asphalt binder used in paving.

Elvoy® 4170 is the most chemically reactive of the terpolymers manufactured by DuPont for use with asphalt. It is effective when used with a wide range of asphalts, at mix levels as low as 1-2%.

Resulting polymer modified asphalt (PMA) is very stable, and can be stored for extended periods.

Availability: Globally

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.577 g/cc
Density 0.940 g/ccASTM D792 - ISO 1183
Melt Flow 5.0 - 11 g/10 minASTM D1238 - ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 72.0 °CASTM D3418 - ISO 3146

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Elvaloy® AM Reactive Ethylene Terpolymer (RET)
Dow Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer
Dow Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer
Dow Elvaloy® AC 1330 Ethylene Methyl Acrylate
Dow Elvaloy® HP662 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer

PDUPM035 / 33702

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.