MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik Kanthal R63C Resistance Heating Wire and Strip
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: R63C is a nickel alloy with high melting point and good conductivity. The alloy is characterized by a low discharge potential as well as good corrosion resistance in carburizing and sulphudizing atmospheres. R63C is typically used for spark plug electrodes.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.72 g/cc0.315 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 440 - 1200 MPa63800 - 174000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000220 ohm-cm0.0000220 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.2 µm/m-°C
@Temperature 20.0 - 500 °C
8.44 µin/in-°F
@Temperature 68.0 - 932 °F
Thermal Conductivity 38.5 W/m-K
@Temperature 100 °C
267 BTU-in/hr-ft²-°F
@Temperature 212 °F
Melting Point 1430 °C2610 °F
 
Component Elements PropertiesMetricEnglishComments
Manganese, Mn 4.0 %4.0 %
Nickel, Ni 95 %95 %
Silicon, Si 1.0 %1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); ST 1550°F (843°C) + Aged at 593°C
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); ST 1550°F (843°C) + Aged at 538°C
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Overaged
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Annealed Strip/Sheet
Armacell FR100 PET Foam

NSANDV5043 / 199607

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.