MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2099 X 144659 EG PC/PBT; ESD Protection - Electrically Conductive - Extrusion Grade
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polyester, TP; Polybutylene Terephthalate (PBT)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.28 g/cc1.28 g/ccASTM D 792
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.126 in
ASTM D 955
Melt Flow 30 g/10 min
@Load 1.20 kg
30 g/10 min
@Load 2.65 lb
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 62.1 MPa9000 psiASTM D 638
Elongation at Break 4.0 - 7.0 %4.0 - 7.0 %ASTM D 638
Tensile Modulus 2.76 GPa400 ksiASTM D 638
Flexural Strength 103 MPa15000 psiASTM D 790
Flexural Modulus 3.10 GPa450 ksiASTM D 790
Izod Impact, Notched 2.14 J/cm
@Thickness 3.20 mm
4.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
NB
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1000 ohm-cm<= 1000 ohm-cmASTM D 257
Surface Resistivity per Square <= 1e+05<= 1e+05ASTM D 257; ESD STM11.11
 
Processing PropertiesMetricEnglishComments
Melt Temperature 243 - 277 °C470 - 530 °F
Drying Temperature 121 °C
@Time 14400 sec
250 °F
@Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 2099 X 147365 PC/PBT; ESD Protection - Permanently Static Dissipative - UV Stabilized - Preliminary Datasheet
RTP Company RTP 2099 X 144676 A Polycarbonate/PBT Alloy (PC/PBT); ESD Protection - Permanently Anti-static - Glass Fiber - Flame Retardant - Preliminary Datasheet
RTP Company RTP 2099 X 144672 Polycarbonate/PBT Alloy (PC/PBT); ESD Protection - Carbon Fiber - Impact Modified - UV Stabilized - Preliminary Datasheet
RTP Company RTP 2099 X 143976 D PC/PBT; Impact Modified - Flame Retardant - UV Stabilized
RTP Company RTP 2099 X 141397 PC/PBT; ESD Protection - Permanently Static Dissipative - Flame Retardant - PTFE Lubricated - UV Stabilized - Preliminary Datasheet

PQZRA35799 / 205948

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.