MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

ITW Chockfast® PHILLYBOND Orange Epoxy Paste
Categories: Polymer; Thermoset; Epoxy

Material Notes: PHILLYBOND ORANGE is a two component, epoxy paste, developed for sealing exposed edges of CHOCKFAST in stern tube applications. It is resistant to sea water and lubricating oils. It has good adhesive strength and flexibility over a wide temperature range. Because of its paste-like consistency, it can be applied in thick, vertical applications without sagging, yet is easy to trowel and provide a smooth finished surface.

USE & BENEFITS: Excellent for sealing any type gap where both mechanical and thermal expansion and contraction will take place. It adheres well to steel, brass, and other epoxies and epoxy chocking materials.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity >= 464000 cP>= 464000 cPMixed. paste consistency
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 4.41 MPa640 psiASTM D638
Elongation at Break 37.5 %37.5 %
Adhesive Bond Strength 2.92 MPa424 psiLap shear vs. steel; ASTM D1002
 3.45 MPa500 psion brass
 3.88 MPa563 psion Chockfast Orange
 3.91 MPa567 psion steel
 
Processing PropertiesMetricEnglishComments
Cure Time  2160 min
@Temperature 21.0 °C
36.0 hour
@Temperature 69.8 °F
Gel 5 hours
 2880 min
@Temperature 15.0 °C
48.0 hour
@Temperature 59.0 °F
Gel 7 hours
Pot Life 180 min
@Temperature 21.1 °C
180 min
@Temperature 70.0 °F
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Coloramberhardener
 orangeresin
 orangemixed
Mix Ratio by volume1 to 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWC9036 / 239546

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.