MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Borealis HE1973 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: HE1973 is a high molecular weight (HMW), high-density polyethylene powder for sheet applications. It offers good impact strength and high stiffness. It is delivered in powder form with good particle size distribution and bright white color. The material is stabilized for transport and storage.

Applications: HE1973 is suitable for compression molding and extrusion of sheets.

Additives: HE1973 is stabilized for transport and storage only.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.958 g/ccISO 1183
Molecular Weight >= 300000 g/molASTM D4020
Melt Flow 3.30 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
Storage Temperature <= 50.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63.0
@Time 15.0 sec
ISO 868
Tensile Strength, Yield 28.0 MPa50 mm/min; ISO 527-2
Elongation at Break >= 600 %ISO 527-2
Tensile Modulus 1200 MPaISO 527-2
Charpy Impact, Notched 65.0 kJ/m²
@Temperature -20.0 °C
ISO 179/1eA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9792 / 323149

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.