Nucleated, good dimensional stability. Produced without animal derived components Sterilization: EtO and autoclave Applications: Irrigation bottles, caps, and closures Regulatory: FDA – 21 CFR 177.1520(c) 3.2a; USP <88> Class VI, USP<85>, and ISO 10993-5 all pending Information provided by INVISTA. |