MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ravago Manufacturing Americas Hylon® N1000MDHL BK Nylon 66, Heat Stabilized, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized; Nylon 66, MoS2 Filled

Material Notes: Product Description: PA 66, Unfilled, Heat Stabilized, Molybdenum Disulfide Lubricant, Black Color

Availability: North America

Additive: Heat Stabilizer; Molybdenum Disulfide Lubricant

Features: Heat Stabilized; Lubricated

RoSH Compliance: RoSH Compliant

Appearance: Black

Information provided by Ravago Manufacturing Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Water Absorption 1.3 %
@Time 86400 sec
1.3 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.014 - 0.018 cm/cm
@Thickness 3.17 mm
0.014 - 0.018 in/in
@Thickness 0.125 in
ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 73.1 MPa10600 psiISO 527-2
Elongation at Break 25 %25 %ISO 527-2
Flexural Strength 114 MPa16500 psiISO 178
Flexural Modulus 3.00 GPa435 ksiISO 178
Izod Impact, Notched (ISO) 6.93 kJ/m²3.30 ft-lb/in²ISO 180
Charpy Impact, Notched 0.693 J/cm²3.30 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 241 °C466 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 92.8 °C199 °FUnannealed; ISO 75-2/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAVAGO4873 / 311566

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.