MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chevron Phillips Marlex® 5335 Low Density Polyethylene, Blown Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: This LDPE is tailored for blown film applications that require:
  • Good processability
  • Low coefficient of friction
  • Good openability
  • Good sealability

Typical blown film applications include:

  • Institutional packaging
  • Food packaging
  • Converter films

Information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.926 g/cc0.926 g/ccASTM D1505
Water Vapor Transmission 15.5 g/m²/day0.998 g/100 in²/dayASTM F1249
Oxygen Transmission Rate 6000 cc/m²/day386 cc/100 in²/dayASTM D3985
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 2750 ppm2750 ppm
Slip Level 750 ppm750 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 330 %330 %ASTM D882
Film Elongation at Break, TD 560 %560 %ASTM D882
Coefficient of Friction 0.120.12ASTM D1894
Elmendorf Tear Strength, MD 9.45 g/micron240 g/milASTM D1922
Elmendorf Tear Strength, TD 9.06 g/micron230 g/milASTM D1922
Dart Drop 2.56 g/micron65.0 g/milASTM D1709
Film Tensile Strength at Break, MD 23.0 MPa3340 psiASTM D882
Film Tensile Strength at Break, TD 20.0 MPa2900 psiASTM D882
1% Secant Modulus, MD 228 MPa33000 psiASTM D882
1% Secant Modulus, TD 255 MPa37000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 7.0 %7.0 %ASTM D1003
Gloss 110 %110 %at 60°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 7308FK Polyethylene; LLDPE
Chevron Phillips Marlex® 5563 LDPE High Clarity, Medium Impact Film Resin
Chevron Phillips Marlex® 5440 Low Density Polyethylene, Cast Film
Chevron Phillips Marlex® D143FK Metallocene Linear Low Density Polyethylene, Blown Film
Dow ELITE™ 5401G Enhanced Polyethylene Resin

PCHEVC903 / 130386

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.