MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Stratasys® RGD4510-DM
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: PRIMARY MATERIAL: DURUSWHITE™ RGD430

SECONDARY MATERIAL: VEROWHITEPLUS RGD835, VEROBLUE RGD840, VEROBLACKPLUS RGD875 OR RGD720

Information provided by Stratasys

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30.0 - 40.0 MPaASTM D638-03
Elongation at Break 40 - 50 %ASTM D638-05
Modulus of Elasticity 1.20 - 1.60 GPaASTM D638-04
Flexural Strength 40.0 - 50.0 MPaASTM D790-03
Flexural Modulus 1300 - 1700 MPaASTM D790-04
Izod Impact, Notched 35.0 - 45.0 J/mASTM D256-06
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 40.0 - 45.0 °CASTM D648-06

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Stratasys® RGD7230-DM Rigid Transparent Digital Material
Stratasys® RGD7220-DM Rigid Transparent Digital Material
Stratasys® RGD4710-DM
Stratasys® RGD4410-DM

PSTRAT143 / 206240

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.